Ürün ayrıntıları:
|
| yapıştırma tipi: | Zift Emdirilmiş | Görünür Gözeneklilik: | % 6 |
|---|---|---|---|
| MgO İçeriği: | %75 | Yığın yoğunluğu: | 3,01 g/cm3 |
| Soğuk kırma gücü: | 42 MPa | Yük altında refrakterlik: | 1690°C |
| Sabit Karbon İçeriği: | %14 | ||
| Vurgulamak: | C14 AOD Cone Brick,Oxidation Resistant Unit,Decarburization Vessel Lining |
||
For AOD cone section duty in a AOD refining vessel, these C14 bricks combine 75% MgO with 14% carbon and a pitch impregnated matrix that resists spalling during AOD decarburization. Carbon content is held at 14% because that is the level where thermal conductivity, slag wetting and oxidation loss stay in balance for AOD decarburization. Apparent porosity of 6% keeps liquid slag from reaching the brick interior, while a cold crushing strength of 42 MPa supports the mechanical
İlgili kişi: Mr. Pika
Tel: 86-13838387996
Faks: 86-0371-56010932